Standard TPU (90A–98A) print settings

Standard TPU (90A–98A) prints at about 225 °C with a 45 °C bed and 30% part cooling. Usable range 210–240 °C nozzle, 25–60 °C bed. No enclosure needed.

TPU 95ATPU 98ATPU 90AFlexibleThermoplastic PolyurethaneMedium TPU

Starting settings

Nozzle
210–240 °C (start 225)
Bed
25–60 °C (start 45)
Part fan
0–50% (start 30%)
Wall speed
10–30 mm/s
Max volumetric flow
3.5 mm³/s
Shrinkage
0.6%
Softens at
-35 °C
Enclosure
Not needed
Nozzle size
0.4 mm or larger — 0.4 mm recommended
Nozzle material
Brass is fine
Drying
50 °C for 6 h

Speed

MUCH SLOWER — 15–30 mm/s, and this is the single most important setting on this material. Above roughly 30 mm/s the filament buckles in the drive gear instead of feeding, and no other change fixes it.

Bed surface

Clean smooth PEI, no adhesive needed — TPU grips well on its own at 45 °C.

Nozzle

0.4 mm is fine. A larger nozzle helps, since flexible filament resists being forced through a small opening.

What bites people

Safety

Open First Layer →
The app walks this in order, generates the test model for your nozzle and filament, and records what you measure so nothing has to be repeated. Free, no account, works offline.