PLA+ / Tough PLA print settings

PLA+ / Tough PLA prints at about 220 °C with a 60 °C bed and 90% part cooling. Usable range 205–235 °C nozzle, 55–70 °C bed. No enclosure needed.

PLA ProPLA MaxTough PLADual-Colour PLA+Multi-Colour PLA+

Starting settings

Nozzle
205–235 °C (start 220)
Bed
55–70 °C (start 60)
Part fan
60–100% (start 90%)
Wall speed
30–60 mm/s
Max volumetric flow
12 mm³/s
Shrinkage
0.3%
Softens at
60 °C
Enclosure
Not needed
Nozzle size
0.2 mm or larger — 0.4 mm recommended
Nozzle material
Brass is fine
Drying
45 °C for 4 h

Speed

Same speeds as plain PLA, 40–60 mm/s. If walls look starved when you speed up, raise temperature before you lower speed — under-extrusion at pace is almost always heat.

Bed surface

Same as PLA. Smooth or textured PEI at 60 °C.

What bites people