Matte PLA print settings

Matte PLA prints at about 215 °C with a 60 °C bed and 100% part cooling. Usable range 200–230 °C nozzle, 55–65 °C bed. No enclosure needed.

Matt PLANon-glossy PLADual-Colour MatteMulti-Colour Matte

Starting settings

Nozzle
200–230 °C (start 215)
Bed
55–65 °C (start 60)
Part fan
80–100% (start 100%)
Wall speed
30–55 mm/s
Max volumetric flow
11 mm³/s
Shrinkage
0.3%
Softens at
60 °C
Enclosure
Not needed
Nozzle size
0.4 mm or larger — 0.4 mm recommended
Nozzle material
Brass is fine
Drying
45 °C for 4 h

Speed

Marginally slower than plain PLA, 30–55 mm/s. The mineral filler makes it less forgiving of high flow, so back off before you reach for a bigger temperature.

Bed surface

Textured PEI suits it — the finish is matte anyway, so a textured bottom looks intentional.

What bites people

Safety

Open First Layer →