High-Flow PETG print settings
High-Flow PETG prints at about 245 °C with a 80 °C bed and 40% part cooling. Usable range 230–260 °C nozzle, 70–90 °C bed. No enclosure needed.
PETG-HFRapid PETG
Starting settings
- Nozzle
- 230–260 °C (start 245)
- Bed
- 70–90 °C (start 80)
- Part fan
- 20–60% (start 40%)
- Wall speed
- 30–80 mm/s
- Max volumetric flow
- 14 mm³/s
- Shrinkage
- 0.4%
- Softens at
- 80 °C
- Enclosure
- Helps
- Nozzle size
- 0.4 mm or larger — 0.6 mm recommended
- Nozzle material
- Brass is fine
- Drying
- 65 °C for 6 h
Speed
FASTER than plain PETG, 45–80 mm/s, IF the hotend can melt it. Same caveat as high-speed PLA: the filament raises its own limit, not your printer's.
Bed surface
Textured PEI, or glue stick on smooth as a release agent.
Nozzle
0.6 mm to actually use the extra flow. On 0.4 mm it prints much like ordinary PETG.
What bites people
- Same caveat as high-speed PLA: the filament melts faster, your hotend still sets the ceiling. Run the flow ramp before trusting the marketing.
- Everything else about PETG still applies — it bonds hard to smooth PEI, and it strings when wet.
Safety
- Nozzle above 230 °C. Bed above 70 °C is hot enough to burn.